Quick answer
- Mild steel, MIG: ER70S-6 solid wire is the everyday choice. Its extra deoxidizers handle light mill scale.
- Mild steel, stick: 6010 or 6011 for dirty, rusty or root passes; 6013 for light, thin work; 7018 for strong, low-hydrogen welds on structural repairs.
- Stainless: 308L for 304, 316L for 316, and 309L when joining stainless to mild steel.
- Aluminum: 4043 for general repair and many 6061 parts; 5356 for marine 5xxx alloys and where strength or anodize color match matters.
- Cast iron: nickel rod (ENi-CI, often called 99 nickel) for machinable repairs, nickel-iron (ENiFe-CI, often called 55 nickel) for thicker sections and cast iron to steel.
How to read the numbers
Stick rod, for example E7018: E means electrode. The first two digits are the minimum tensile strength of the weld metal in thousands of psi, so 70 means 70,000 psi. The third digit is position: 1 means all positions. The last digit describes the coating and the current it runs on. That is why 6010 and 6011 behave alike except that 6011 runs on AC, and why 7018 is low hydrogen.
Solid wire and rod, for example ER70S-6: ER means it can be used as an electrode (MIG) or a rod (TIG). 70 is strength in thousands of psi. S means solid. The 6 refers to the chemistry, with more manganese and silicon deoxidizers than ER70S-3.
Flux-core, for example E71T-11 or E71T-GS: T means tubular. The suffix tells you whether it is self-shielded and whether it is rated for single pass or multiple passes. GS wires are for single-pass welds only, which matters on thicker repairs.
Steel: stick rods
| Rod | Best for | Notes |
|---|---|---|
| E6010 | Deep penetration, dirty or rusty steel, pipe root passes | DC only. Fast-freezing, good out of position. Rough looking. |
| E6011 | Same jobs on an AC machine | The farm repair rod for buzz boxes. Digs through rust and paint better than most. |
| E6013 | Thin steel, light-duty and cosmetic work | Easy to strike, smooth bead, shallow penetration. Not for heavy structural repairs. |
| E7018 | Strong structural repairs: hitches, frames, equipment | Low hydrogen. Store dry, ideally in a rod oven once opened. Needs clean metal. |
| E7014 | Fast fill in flat and horizontal welds | Smooth and easy, less common for repair. |
Steel: wire
- ER70S-6 with 75/25 argon-CO2: the default MIG setup for mild steel. Pure CO2 also works, with more spatter and deeper penetration.
- Self-shielded flux-core (E71T-11, E71T-GS and similar): no gas, works outdoors. Check whether your wire is rated for multiple passes before using it on thick repairs.
- Gas-shielded flux-core (E71T-1 and similar): high deposition and good penetration in fabrication shops. Needs gas and a bigger machine.
Wire diameter follows thickness and machine size. Our Welding Settings Calculator suggests wire size, amps and voltage from published maker charts.
Stainless steel
- 308L: for 304 and 304L stainless. The L means low carbon, which helps the weld resist corrosion.
- 316L: for 316 stainless, common in marine, food and chemical equipment.
- 309L: for joining stainless to mild steel. Its extra alloy handles dilution with the carbon steel. See stainless to mild steel.
Stainless MIG uses a gas mix made for stainless, and TIG uses argon. More in Can stainless steel be welded?
Aluminum: 4043 vs 5356
| 4043 | 5356 | |
|---|---|---|
| Alloying | Silicon | Magnesium |
| Strengths | Flows well, less prone to cracking on many 6061 and cast parts | Stronger, stiffer wire that feeds better in a MIG gun |
| Common use | General repair, castings, 6061 | Marine 5052, 5083 and 5086, trailers, parts to be anodized |
| Avoid | High-magnesium 5xxx hull plate | Some high-silicon castings |
Neither one restores full strength to heat-treated 6061-T6 next to the weld. See Can aluminum be welded? and cast aluminum.
Cast iron
- ENi-CI (99 nickel): soft, machinable deposit. Good for thin to moderate castings and repairs that need drilling or machining afterward.
- ENiFe-CI (55 nickel): stronger, better on thicker castings, ductile iron, and cast iron to steel.
- Steel rod on cast iron: usually a mistake. It makes a hard, brittle zone that cracks.
- Bronze brazing rod: for braze welding, covered in brazing vs welding.
Specialty fillers
- Silicon bronze (ERCuSi-A): MIG or TIG brazing of galvanized and thin steel, and some copper and brass work.
- Hardfacing rods and wires: build up wear surfaces on bucket edges, tillage points and teeth. They are hard and not for joining parts.
- Chromoly: ER70S-2 and ER80S-D2 are common choices for 4130 tubing, depending on the job and the maker's guidance. See chromoly.
Storage and handling
Filler is only as good as its condition. Keep stick rod sealed and dry, and keep low-hydrogen rod like 7018 in a rod oven once the can is opened, because a damp coating puts hydrogen into the weld. Keep MIG wire covered so it does not rust. Keep TIG rods in a closed tube and wipe them before use. Mark aluminum and stainless brushes and keep them away from steel to avoid contamination.
Not sure what the base metal is? Start with how to identify metal, then check the pairing in the Weldability Checker.
🧰 Tools & parts for this job
The links in the strip at the top of this page are Amazon searches for the gear this job uses. They are paid links (Amazon Associate), not endorsements of a specific product. Links never change a verdict.
⚠️ Safety
- Stainless filler and base metal contain chromium, and welding fume from them needs good extraction.
- Nickel and bronze fillers also produce fume that should not be breathed. Ventilate every process.
- Never weld galvanized parts without removing the zinc at the joint and ventilating, even with bronze filler.
- Read the safety data sheet for any filler you use. It lists fume hazards and protective equipment.
Common questions
What is the best all-around welding rod?
For mild steel, 6011 is the most forgiving all-around rod on an AC machine, especially on dirty metal, while 7018 makes stronger, cleaner structural welds on clean steel. Many welders keep both.
What is the difference between 4043 and 5356?
4043 contains silicon, flows easily and resists cracking on many 6061 and cast parts. 5356 contains magnesium, is stronger, feeds better in MIG guns and suits marine 5xxx alloys and parts that will be anodized.
What rod do I use for cast iron?
Nickel rod: ENi-CI (99 nickel) for machinable repairs on thinner castings, or ENiFe-CI (55 nickel) for thicker castings and cast iron to steel. Avoid steel rod.
What wire welds stainless to mild steel?
309L is the standard choice for joining stainless to carbon steel.
Does 7018 need a rod oven?
Low-hydrogen rods like 7018 should be kept dry. For critical work, opened rods are stored in a heated rod oven. For home repairs, at minimum keep them sealed and dry.