Home › Guides › Metals & Welding Basics › Welding glossary
Welding Glossary: Plain-English Welding and Repair Terms
REFERENCEFifty common welding and repair terms in plain English, linked to the guides where they matter
From CanItBeWelded.com, run by Rick, a working welder at RickTheWelder. Published November 29, 2026. How we write and check guides.
Have a question rather than a term? See the welding repair FAQ.
How to use this glossary
- Terms are listed alphabetically. Each one links to the guide where it matters most when there is one.
- If a guide uses a word you do not know, it is probably here.
- Missing a term? Tell us on the contact page and we will add it.
Terms A to Z
- AC and DC
- Alternating and direct current. Aluminum TIG uses AC to break up oxide; most steel welding uses DC. Some stick rods, like 6011, are made to run on AC machines.
- Arc flash
- A burn to the surface of the eye from welding ultraviolet light, also called welder's flash. Painful, usually felt hours later.
- Back purge
- Filling the back side of a joint, such as the inside of a tube, with shielding gas so the root does not oxidize. Used on stainless and titanium.
- Bevel
- An angle ground on the edge of thick metal so the weld can reach the root of the joint.
- Braze welding
- Building up a bronze bead in a groove without melting the base metal. A common cast iron repair. See brazing vs welding.
- Brazing
- Joining metal with a filler that melts above about 840 °F without melting the base metal.
- Buildup
- Weld metal laid down to restore worn dimensions before hardfacing or machining.
- Burn-through
- A hole melted through thin metal by too much heat.
- Carbon equivalent
- A number combining a steel's carbon and alloy content, used to judge how likely it is to crack when welded and how much preheat it needs.
- Cast iron
- Iron with a high carbon content, poured into molds. Brittle and crack-prone when welded. See cast iron.
- Cold lap
- Weld metal that rolls over the surface without fusing into it. Looks fine, holds poorly.
- Crater crack
- A small crack at the end of a bead where the puddle shrank as it froze. Prevented by filling the crater.
- Duty cycle
- How many minutes out of ten a welder can run at a given output before it needs to cool.
- Distortion
- Warping caused by weld shrinkage as it cools.
- Electrode
- The rod or wire that carries welding current. In stick and MIG it also becomes filler; in TIG the tungsten electrode does not melt.
- Filler metal
- Rod or wire added to the joint. See the rod and wire guide.
- Fillet weld
- A triangular weld joining two surfaces at an angle, such as a T joint or lap joint.
- Fit-up
- How well parts are aligned and gapped before welding.
- Flux
- A material that shields or cleans the weld or braze. It coats stick rods, fills flux-core wire, and is applied separately for brazing.
- Flux-core (FCAW)
- Wire welding with a tubular wire filled with flux. Self-shielded types need no gas.
- Fusion
- The melting together of base metal and filler. Lack of fusion is a common hidden defect.
- Galvanized
- Steel coated with zinc for corrosion protection. The zinc must be removed from the weld area. See galvanized steel.
- Gas lens
- A TIG torch part that smooths gas flow for better shielding coverage.
- Ground clamp (work clamp)
- The clamp that completes the welding circuit. Place it on clean metal close to the weld.
- Hardfacing
- Applying a hard, wear-resistant weld deposit to surfaces like bucket edges and tillage tools.
- Heat-affected zone (HAZ)
- Base metal next to the weld that did not melt but was changed by the heat. Often where cracks start.
- Hydrogen cracking
- Cracks caused by hydrogen trapped in hard metal near a weld, sometimes appearing hours later. Also called cold or delayed cracking.
- Interpass temperature
- The temperature of the part between weld passes, kept within a range on critical work.
- Low hydrogen
- Filler, such as E7018, made to put very little hydrogen into the weld. Must be kept dry.
- Metal fume fever
- Flu-like illness from breathing metal oxide fume, most often zinc from galvanized steel.
- MIG (GMAW)
- Gas metal arc welding with solid wire and shielding gas.
- Mill scale
- The dark, flaky oxide on hot-rolled steel. Best removed before welding.
- Multi-pass
- A weld built up in several layers: root, fill and cap passes.
- Nickel rod
- Filler with high nickel content used on cast iron because it stays ductile.
- Peening
- Lightly hammering a hot weld bead to relieve shrinkage stress, often used on cast iron.
- Penetration
- How deep the weld fuses into the joint.
- Porosity
- Gas holes in a weld, usually from contamination or lost shielding gas.
- Pot metal
- Low-melting zinc-based die cast alloy, often chrome plated. Very hard to weld. See pot metal.
- Preheat
- Heating the part before welding to slow cooling and prevent cracking. See when to preheat.
- Root
- The deepest part of a joint, where the first pass goes.
- Shielding gas
- Gas that protects the molten weld from air, such as argon, CO2 or mixes of the two.
- Slag
- The glassy crust left by flux on stick and flux-core welds. Must be removed between passes.
- Spatter
- Molten droplets thrown from the arc that stick to nearby surfaces.
- Spool gun
- A MIG gun with a small wire spool on the gun itself, used to feed soft aluminum wire.
- Stick (SMAW)
- Shielded metal arc welding with flux-coated rods.
- Stop hole
- A small hole drilled just past the end of a crack to keep it from spreading.
- Tack weld
- A short weld that holds parts in position before the full weld.
- TIG (GTAW)
- Gas tungsten arc welding with a non-melting tungsten electrode, argon and hand-fed filler.
- Toe of the weld
- Where the weld face meets the base metal. A common place for fatigue cracks to start.
- Undercut
- A groove melted into the base metal along the weld edge and left unfilled.
- Weldability
- How easily a metal can be welded with sound results. Check pairs in the Weldability Checker.
Want to put the terms to work? Start with MIG vs TIG vs stick and how to prep metal for welding.
⚠️ Safety
- Definitions here are general. Follow the instructions for your machine, filler and the part you are repairing.
- Read the welding safety guide before you weld.