Home › Tools › Weldability Checker

Weldability Checker: Can These Two Metals Be Welded Together?

Pick two metals. The checker tells you whether they can be welded together, which process works, what filler rod or wire to use, how to prep and preheat, and what usually goes wrong. It covers 20 common metals and every pairing between them.

General guidance from common shop practice and filler makers' recommendations, not a welding procedure. Exact alloy, thickness and the job change the answer. Check your filler maker's data sheet, and use a qualified procedure for code, structural or pressure work. Not sure what metal you have? See how to identify metal.

How to read the result

Common pairings

Stainless steel 304 + Mild steel (low-carbon)

Yes Yes. Stainless is commonly welded to carbon steel with 309 or 309L filler.

Filler: TIG: ER309L. MIG: ER309L or ER309LSi. Stick: E309L-16. Do not use mild-steel filler or 308L for this joint.

Guide: Can stainless be welded to mild steel? Can you weld stainless steel?

Aluminum (sheet, plate, extrusion) + Mild steel (low-carbon)

Not practical Not with a normal arc weld. Aluminum and steel form a brittle intermetallic layer that cracks. Use a bimetal transition insert (weld each metal to its own side) or bolt or rivet the parts.

Filler: Only with a bimetal transition insert: aluminum filler (ER4043/ER5356) to the aluminum face, steel or stainless filler to the steel face. Never weld across the bond line.

Guide: Can aluminum be welded to steel? Can aluminum be welded?

Gray cast iron + Mild steel (low-carbon)

Yes, with caveats Yes with care. Cast iron to steel is usually welded with nickel-iron rod, or brazed with bronze rod for lower-stress joints.

Filler: Stick: ENiFe-CI (about 55% nickel) is the usual choice for cast iron to steel. TIG: ERNi-CI. Brazing: bronze rod such as RBCuZn-C or silicon bronze.

Guide: Cast iron repair

Galvanized steel to itself

Yes, with caveats Yes, after the zinc coating is removed from the weld area and with real ventilation; recoat the weld afterward.

Filler: Mild-steel fillers once the zinc is off (ER70S-6, E6011, E7018). On thin galvanized sheet, silicon bronze (ERCuSi-A) MIG or TIG brazing is also used because it runs cooler.

Guide: Can you weld galvanized steel?

Aluminum (sheet, plate, extrusion) to itself

Yes, with caveats Yes, by a welder set up for aluminum: AC TIG, or MIG with a spool or push-pull gun and 100% argon. Heat-treated parts lose strength at the weld.

Filler: ER4043 or ER5356, chosen by the base alloy (5356 is usual for 5xxx alloys; either is common on 6061). 7075 and 2024 aircraft alloys are poor candidates for welding.

Guide: Can aluminum be welded?

Gray cast iron to itself

Yes, with caveats Often yes, with the right method: preheat and nickel rod, or brazing. Done wrong, it cracks right beside the repair.

Filler: Stick: ENi-CI (about 99% nickel, softest and most machinable) or ENiFe-CI (about 55% nickel, stronger). Brazing: bronze rod such as RBCuZn-C, or silicon bronze.

Guide: Cast iron repair

Chromoly (4130) + Mild steel (low-carbon)

Yes, with caveats Yes. Chromoly and mild or low-alloy steel are commonly welded together with a mild-steel filler; the joint is only as strong as the weaker side.

Filler: TIG: ER70S-2 or ER70S-6. MIG: ER70S-6. Stick: E7018 (low-hydrogen).

Guide: Can chromoly (4130) be welded?

Stainless steel 304 + Stainless steel 316

Yes Yes. 304 and 316 are routinely welded together.

Filler: ER308L or ER316L (316L if the corrosion resistance of the 316 side matters). Stick: E308L-16 or E316L-16.

Guide: Can you weld stainless steel?

Copper + Brass

Yes, with caveats Yes, by brazing. Copper to brass is a standard brazed or soldered joint in plumbing and fittings.

Filler: Copper-phosphorus rod works copper to brass with flux on the brass side; silicon bronze (ERCuSi-A) for TIG brazing.

Guide: Can copper be welded? Can brass be welded?

Copper + Mild steel (low-carbon)

Yes, with caveats Yes, usually by brazing rather than fusion welding. Copper to mild steel is normally brazed or braze-welded with silicon bronze.

Filler: Silicon bronze (ERCuSi-A) for TIG or MIG brazing, or bronze rod (such as RBCuZn-C) with flux for oxy-fuel brazing. A true fusion weld of copper to steel uses nickel-copper filler and is specialist work.

Guide: Can copper be welded?

High-carbon / hardened steel + Mild steel (low-carbon)

Yes, with caveats Yes, with care. Preheat for the high-carbon side, low-hydrogen filler and a slow cool. The joint is only as strong as the weaker side, and the hard steel will not stay hard at the weld.

Filler: Dry low-hydrogen filler such as E7018 or a low-hydrogen wire. Some shops use 312-type stainless or nickel rod when the hard steel is unknown or crack-prone.

Guide: Can hardened steel be welded?

Pot metal / zinc die-cast to itself

Not practical Usually not with a normal welder. Low-temperature zinc repair rods can work on some parts in skilled hands; most broken pot metal is replaced or epoxied if non-structural.

Filler: Low-temperature zinc-aluminum repair rod with a small torch (a low-temperature braze, not an arc weld). Steel-reinforced epoxy for non-structural parts.

Guide: Can pot metal be welded?

Cast aluminum to itself

Yes, with caveats Often yes on clean sand-cast parts; often no on porous, oil-soaked die-castings. Identify the part first.

Filler: ER4043 is common on high-silicon cast alloys such as 356/A356; the right filler depends on the alloy.

Guide: Can cast aluminum be welded?

Brass + Mild steel (low-carbon)

Yes, with caveats Yes, usually by brazing rather than fusion welding. Brass to mild steel is normally brazed or braze-welded with silicon bronze.

Filler: Silicon bronze (ERCuSi-A) for TIG or MIG brazing, or bronze rod (such as RBCuZn-C) with flux for oxy-fuel brazing.

Guide: Can brass be welded?

Frequently asked questions

How do I know if two metals can be welded together?

Pick both metals in the checker. Metals from the same family, like mild steel and low-alloy steel, usually weld together with ordinary filler. Very different metals, like aluminum and steel, form brittle compounds when melted together and usually have to be joined another way.

What filler do I use to weld stainless steel to mild steel?

A 309L filler is the standard choice: ER309L or ER309LSi wire for MIG and TIG, or an E309L-16 stick rod. Do not use mild steel filler or 308L for this joint.

Can aluminum be welded to steel?

Not with an ordinary MIG, TIG or stick weld. The two metals form brittle compounds and the joint cracks. Shops use a bimetal transition insert, bolts or rivets, or a specialist process instead.

What rod do you use to weld cast iron to steel?

A nickel-iron rod such as ENiFe-CI is the usual stick choice for joining cast iron to steel. Brazing with bronze rod is another common option when the part does not need full weld strength.

Can galvanized steel be welded?

Yes, but the zinc coating has to be ground off the weld area first and the zinc fumes are a real health hazard. Work with strong ventilation or a respirator and coat the bare area with cold galvanizing paint afterward.

Is this checker a welding procedure?

No. It gives general guidance based on common shop practice and the filler makers' recommendations. Exact alloys, thickness and the job change the answer, so check your filler maker's data sheet, and follow a qualified procedure for code, structural or pressure work.